Practices and solutions to prevent MLCC fracture damage

Share this article

LinkedIn
Twitter

In any modern electronic design, multilayer ceramic capacitors (MLCCs) are indispensable components. Compact and inexpensive, they are integrated into hundreds of everyday applications and devices, from a switching power supply (SMPS) to an automotive ECU. However, beneath this apparent robustness hides one of the most common – and often unnoticed – failure modes in the electronics industry: MLCC fracture.

This type of failure, generated by mechanical or thermal stresses accumulated during assembly and/or application, can severely compromise system operation, causing anything from performance drops to catastrophic short circuits.

Fortunately, advances in encapsulation technologies, on-board orientation and internal design of SMD ceramic capacitors make it possible to prevent these fractures or, failing that, to ensure that they do not lead to critical failures.

In this article we explore how to understand and mitigate this risk, analyzing possible solutions and sharing key recommendations to maximize the reliability of your circuits to avoid incurring damage from an MLCC failure. The unit price of a ceramic capacitor is generally very low, but the damage resulting from its failure can escalate to non-negligible magnitudes.

What is a MLCC?

To understand why the fracture of an MLCC can become critical for the system, we must first understand its internal structure. These types of capacitors are layered inside by multiple layers of metal electrodes (often nickel), alternating with the dielectric material (in this case, ceramic). This design, despite providing the favorable characteristics that have propelled its use and ubiquity, also give it a great weakness: the fragile nature of the ceramic, susceptible to accumulate stresses that can lead to partial cracks or fractures of the component.

Que-es-un-MLCC-2_en

Why is fracking critical?

When mechanical or thermal stresses accumulate in an MLCC, they can lead to a fracture that usually originates at the end of the capacitor and propagates inward. Three scenarios can be distinguished:

  • The first, and most serious, occurs when the fracture crosses two electrodes of opposite polarity. In such a case, we will find an internal short circuit.
  • The second, less delicate, but equally worrying, is when opposite electrodes are not connected. In this case, we can have:
    • Functional degradation: loss of nominal capacity.
    • Increase of the equivalent series resistance (ESR).
    • Insulation resistance drop (IR).
  • Finally, in some occasions we can visualize a superficial crack. Small superficial microcracks are potential internal fractures, as well as being the capillary channel for the entry of moisture and contamination, as well as a possible cause of irregularities in the electric fields, sometimes even producing the arcing effect.
Fractura 1

Most frequent reasons for fracture of the MLCC

  1. Board Bending

Plate bending is the main cause of mechanical failure of large case size MLCCs. A single one-millimeter bend can be enough to fracture a 1206 MLCC.

Bending can occur when depaneling or handling the PCB, connecting/disconnecting rigid connectors, mounting screw-in modules or inserting the board into a housing, among other possibilities. Long PCBs are by far more susceptible to bending.

There are a number of considerations and good design practices that minimize the risk of stress accumulation in MLCCs during the assembly and depaneling process. In general, it is advisable to place the ceramic capacitors respecting safety margins with the edges, but if it is unavoidable, certain aspects must be taken into account.

  • If the edge is milled, low stresses are introduced and, therefore, the threat of fracture will also be lower.
  • If it is V-scoring edge, the stresses induced when separating the PCB’s cause a bending perpendicular to the shear plane, so the longitudinal direction of the MLCC must be collinear with the shear line.
  • In tab-routing areas, MLCCs should be moved as far away as possible by establishing exclusion zones.
  1. Thermal stresses (reflow and thermal cycling)

During reflow soldering, MLCCs experience a strong thermal gradient that can induce internal stresses due to differential expansion.

If the MLCC is not cooled evenly, micro-cracks may appear from the corners of the component.

In the field, on/off cycling or use in wide thermal range environments (such as automotive) also induce repetitive stress.

  1. Vibrations and mechanical impacts

In applications such as automotive, machinery or rail transport, prolonged vibration can cause micro-cracking due to accumulated fatigue.

Although the MLCC does not rupture immediately, small cracks may progress until a complete rupture occurs.

How to avoid bending fracture?

Considering the impact of this type of failure, manufacturers developed flexibly terminated MLCCs, currently the most effective method of preventing capacitor fracture without having to modify the design.

It consists of adding a layer of flexible conductive material – usually silver polymer – between the ceramic and the outer conductor terminal, which absorbs mechanical stresses, preventing bending fractures of up to five millimeters. This innovation is highly effective and generally sufficient. But what happens if the working conditions exceed the absorption capacity of this new layer? In that case, additional safety measures are needed to prevent short circuits.

Safe failure strategies: avoiding short-circuit after fracture

In today’s demanding environments, we cannot completely eliminate the risk of fracture. Therefore, manufacturers put the focus on the internal restructuring of MLCCs.

Open Mode Failure Design

This is a configuration in which the internal electrodes do not extend to the opposite edge of the chip, but are held within a “protected” central area.

In case of transverse fracture, the crack is usually formed from the ends of the chip inwards. As the electrodes do not reach that area, the crack cannot connect opposite polarities, so the capacitor partially or completely loses its functionality, but does not cause a short circuit, thus protecting the rest of the components.

Fractura 2

Floating Electrodes Design

The internal architecture of these MLCCs revolutionizes the original concept because we now have two capacitors in series inside the same box. In the event of a breakage, it will not short circuit, although it will partially lose its rated capacity. These MLCCs are most commonly used in safety applications and are designed to comply with X1/Y2 and X2 standards.

Fractura 3

Definitive solution

Since nothing prevented it, manufacturers have combined flexible termination with internal fail-safe structures, offering ideal alternatives for those applications where it is critical to maintain the integrity and safety of the equipment and any operators handling it.

Technical comparative

Criteria
Soft Terminal
Open Mode
Floating Electrode
What does this solve?
Fracture prevention
Minimizing the electrical impact of internal fractures
Avoid short circuits after fracture
Action level
External (chip termination)
Internal (electrode design)
Internal (serial multilayer architecture)
Mechanism
Flexible layer between ceramic and terminal
Internal electrode does not reach the edge of the chip
Intermediate floating electrodes → series sections
Typical failure mode
If fracture: short circuit
If fracture: open circuit
If fracture: reduced capacitance or isolated section
Short circuit protection
Prevents the cause, not the effect
High: design avoids contact between cracked polarities
Very high: electrically decoupled internal sections

Eurotronix, experts in MLCC since 1986

At Eurotronix we offer top quality MLCC ceramic capacitors, manufactured by leading brands in the market. In addition, our Product Manager and FAE team will support you in your projects to offer reliable, safe and adapted solutions to the current challenges of electronics.

Authors

Álvaro Guerris

Ceramic Capacitors Product Manager

Néstor Galera

Electronic components FAE

Share this article

Resumen de privacidad

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team understand which sections of the website you find most interesting and useful.